Studies of the hardness for the sintered tantalum boride (TaB) at high temperature and high pressure
DOI:
Author:
Affiliation:

Clc Number:

O521+.2

Fund Project:

  • Article
  • |
  • Figures
  • |
  • Metrics
  • |
  • Reference
  • |
  • Related
  • |
  • Cited by
    Abstract:

    Tantalum boride has been sintered under high temperature and high pressure (HTHP) conditions by using a DS6×8 MN cubic press device, and the Vickers hardness of TaB has been measured by using a diamond indentation method. Under the applied load of 29.4 N, our test gave the Vickers hardness of TaB are 7.7±0.4 and 10.5±0.7 GPa, at 4 GPa and the temperatures of 900 and 1100 ℃, respectively. Our result shows that the density becomes better with the increasing temperature under the same pressure. By using the Archimedes method, we calculated the relative density of 13.5 g/cm3 for TaB.

    Reference
    Related
    Cited by
Get Citation

Cite this article as: CHEN Hai-Hua, LIANG Hao, XIE Ming-Cai, LIU Ling-Xiao, ZHENG Shu-Dong. Studies of the hardness for the sintered tantalum boride (TaB) at high temperature and high pressure [J]. J Sichuan Univ: Nat Sci Ed, 2017, 54: 835.

Copy
Share
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:April 09,2017
  • Revised:May 01,2017
  • Adopted:May 18,2017
  • Online: July 03,2017
  • Published: