Microstructures and hot compression behavior of Mg-4Sn-1Ce alloy
Author:
Affiliation:

Clc Number:

TG146.2

Fund Project:

  • Article
  • |
  • Figures
  • |
  • Metrics
  • |
  • Reference
  • |
  • Related
  • |
  • Cited by
    Abstract:

    The microstructures and hot compression behavior of Mg-4Sn-1Ce alloy were studied by optical microscopy (OM), X-ray diffraction (XRD), scanning electron microscopy (SEM) and hot simulation test. The results shown that the as-cast alloy is mainly composed of island-like “island” shaped α-Mg、Mg2Sn、Ce4Sn5 and MgSnCe phases with the strain rate range of 0.001~1 s-1 and temperature range of 250~450 ℃ hot compression. The hot deformation activation energy Q is 162.03 kJ/mol. When the hot compression temperature increases from 250 to 450 ℃, the microstructures of tested alloy evolve from (compressed grains+extruded streamlines) to recrystallized equiaxed grains.

    Reference
    Related
    Cited by
Get Citation

Cite this article as: WU Ying, ZENG Qiang, HU Guang-Shan, WEN Tong. Microstructures and hot compression behavior of Mg-4Sn-1Ce alloy [J]. J Sichuan Univ: Nat Sci Ed, 2021, 58: 015001.

Copy
Share
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:May 30,2020
  • Revised:July 09,2020
  • Adopted:August 10,2020
  • Online: January 20,2021
  • Published: